| Property | Test Method | Unit | Value |
| Polymer | | | EPDM |
| Cell Structure | | | Semi-closed |
| Density | ISO 845 | kg/m³ | 115 - 150 |
| Compression Deflection 25% | ISO 6916-1 | kPa | 3 - 5 |
| Compression Deflection 50% | ISO 6916-1 | kPa | 5 - 10 |
| Compression Set 25% | ISO 6916 / ISO 1856 - 23°C/22h/50% | % Max | 5 |
| ISO 6916 / ISO 1856 - 40°C/22h/50% | % Max | 40 |
| Tensile Strength | ISO 1798 | kPa Min | 150 |
| Linear Shrinkage | ISO 2796 24h/70°C | % Max | 5 |
| Ozone Resistance | ISO 1431-1 20% strain / 40°C / 200 pphm | Rating | Excellent |
| Temperature Use | | °C min | -40 |
| | °C max | +120 |
| Maximum Thickness | | mm | 20 |
| Tear Resistance | ISO 34-1 | kN/m Min | 0.9 |
| Dimensional Stability | ISO 2796 3h/80°C | % Max | 5 |
| Water Seal | | | Armacell Test 013 - 75% Compression - 30 |
| UV Resistance | | | Excellent |
| Flammability Rating | FMVSS 302 | | Pass |
| Specification | ASTM D 1056 SAEJ 18 | | 1A0 |